HS Code |
916920 |
| Product Name | Alkyd Conductive Enamel C04-22 |
| Type | Conductive Enamel |
| Binder | Alkyd Resin |
| Color | Black |
| Finish | Semi-gloss |
| Conductivity | High |
| Drying Time Touch | 1-2 hours |
| Drying Time Hard | 8-10 hours |
| Theoretical Coverage | 10-12 m2/L |
| Thinner | Alkyd Thinner |
| Application Method | Brush, Roller, Spray |
| Recommended Dft | 30-40 microns |
| Storage Temperature | 5-35°C |
| Flash Point | Above 37°C |
| Main Use | Electrostatic Protection |
As an accredited Alkyd Conductive Enamel C04-22 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | The Alkyd Conductive Enamel C04-22 is packaged in a durable 5-liter metal can, clearly labeled with product and hazard information. |
| Container Loading (20′ FCL) | Container Loading (20′ FCL): Alkyd Conductive Enamel C04-22 is shipped in 200 kg steel drums, 80 drums per 20′ FCL. |
| Shipping | Alkyd Conductive Enamel C04-22 should be shipped in tightly sealed, corrosion-resistant containers, protected from physical damage, moisture, and heat sources. Label containers with hazard warnings and handle according to local, national, and international chemical transport regulations. Ensure upright storage and proper documentation for safe and compliant delivery. |
| Storage | **Alkyd Conductive Enamel C04-22** should be stored in tightly sealed containers, in a cool, dry, and well-ventilated area away from heat, sparks, open flames, and direct sunlight. Avoid freezing temperatures and sources of ignition. Keep away from incompatible materials such as strong oxidizers and acids. Follow local regulations for storage and ensure proper labeling of all containers. |
| Shelf Life | Alkyd Conductive Enamel C04-22 has a shelf life of 12 months when stored unopened in cool, dry conditions. |
|
Surface Resistivity: Alkyd Conductive Enamel C04-22 with surface resistivity of 10^5 Ω/sq is used in electronic cabinet coatings, where it prevents static charge accumulation. Viscosity Grade: Alkyd Conductive Enamel C04-22 formulated at 90 KU viscosity grade is used in transformer housings, where it ensures uniform film formation and easy spray application. Drying Time: Alkyd Conductive Enamel C04-22 with a drying time of less than 60 minutes is used in assembly line painting, where it enables rapid processing and productivity. Adhesion Strength: Alkyd Conductive Enamel C04-22 rated for 5B adhesion strength is used in busbar protection, where it delivers excellent substrate bonding and minimizes peeling. Stability Temperature: Alkyd Conductive Enamel C04-22 stable up to 120°C is used in motor casing finishes, where it maintains conductivity and physical integrity under thermal stress. Pigment Volume Concentration: Alkyd Conductive Enamel C04-22 with 25% pigment volume concentration is used in telecom enclosure finishing, where it provides effective shielding and color retention. Flexibility: Alkyd Conductive Enamel C04-22 with high flexibility is used in cable tray coatings, where it prevents cracking during handling and installation. Particle Size: Alkyd Conductive Enamel C04-22 with a particle size below 20 μm is used in electronic device interiors, where it ensures smooth surface and consistent conductivity. Salt Spray Resistance: Alkyd Conductive Enamel C04-22 providing 300-hour salt spray resistance is used in outdoor electrical panel coatings, where it enhances corrosion protection. Solids Content: Alkyd Conductive Enamel C04-22 with 55% solids content is used in busbar trunking systems, where it offers high build coverage and efficient shielding. |
Competitive Alkyd Conductive Enamel C04-22 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8615651039172 or mail to sales9@bouling-chem.com.
We will respond to you as soon as possible.
Tel: +8615651039172
Email: sales9@bouling-chem.com
Flexible payment, competitive price, premium service - Inquire now!